Polyram RamLloy PBB520 PC/ABS alloy, Flame Retardant

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Polyram
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamLloy PBB520 PC/ABS alloy, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant PC/ABS alloy for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
DIN 53479
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
Melt Flow 25 g/10 min

@Load 5.00 kg,
Temperature 240 °C
25 g/10 min

@Load 11.0 lb,
Temperature 464 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ASTM-D638
Elongation at Break 25 %
25 %
ASTM-D638
Tensile Modulus 2.20 GPa
319 ksi
ASTM-D790
Izod Impact, Notched 3.50 J/cm

@Temperature 23.0 °C
6.56 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Glow Wire Test 960 °C
1760 °F
Electrical Properties Metric English Comments
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
DIN 53482
Dielectric Strength 24.0 kV/mm
610 kV/in
VDE 0303/4