Material Notes:
PC/ABS alloy for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
DIN 53479
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
Melt Flow 18 g/10 min
18 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
ASTM-D638
Elongation at Break 60 %
60 %
ASTM-D638
Flexural Strength 90.0 MPa
13100 psi
ASTM-D790
Flexural Modulus 2.30 GPa
334 ksi
ASTM-D790
Izod Impact, Notched 4.00 J/cm

@Temperature 23.0 °C
7.49 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
DIN 53461
Vicat Softening Point 120 °C
248 °F
ASTM-D1525
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
DIN 53482
Dielectric Strength 24.0 kV/mm
610 kV/in
VDE 0303/4