Polyram RamLloy PA917G4 PP/NYLON 66 alloy, 20% Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Polypropylene (PP)
Manufacturer Polyram
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamLloy PA917G4 PP/NYLON 66 alloy, 20% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% glass fiber reinforced PA66/PP alloy with reduced water absorption, dimensional stability and UV stabilized for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
DIN 53479
Water Absorption 3.5 %
3.5 %
DIN 53495
Moisture Absorption at Equilibrium 1.5 %
1.5 %
DIN 53714
Linear Mold Shrinkage 0.00 - 0.0050 cm/cm
0.00 - 0.0050 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM-D785
Tensile Strength, Yield 115 MPa
16700 psi
ASTM-D638
Elongation at Break 3.0 %
3.0 %
ASTM-D638
Flexural Strength 195 MPa
28300 psi
ASTM-D790
Flexural Modulus 5.70 GPa
827 ksi
ASTM-D790
Izod Impact, Notched 1.00 J/cm

@Temperature 23.0 °C
1.87 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous Use
150 °C
302 °F
Short peaks operation
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in