Polyram RamClean™ 800 Ethylene Propylene Compound Purging Agent

Category Polymer , Thermoplastic , Purging Compound
Manufacturer Polyram
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamClean™ 800 Ethylene Propylene Compound Purging Agent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ethylene propylene compound purging agent for extruders/injection molding machines.Information provided by Polyram.
Physical Properties Metric English Comments
Melt Flow 7.5 g/10 min

@Load 10.0 kg,
Temperature 230 °C
7.5 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ISO 1133