Polyram Polytron P50N01 Homopolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 50% Glass Fiber Filler
Manufacturer Polyram
Trade Name Polytron
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram Polytron P50N01 Homopolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A CHEMICALLY COUPLED 50% LONG GLASS FIBER REINFORCED NATURAL POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ASTM-D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 135 MPa
19600 psi
ASTM-D638
Elongation at Break 2.0 %
2.0 %
ASTM-D638
Tensile Modulus 13.9 GPa
2020 ksi
ASTM-D790
Flexural Strength 210 MPa
30500 psi
ASTM-D790
Flexural Modulus 11.0 GPa
1600 ksi
ASTM-D790
Izod Impact, Notched 2.50 J/cm

@Temperature 23.0 °C
4.68 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 159 °C
318 °F
ASTM-D648