Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram Polytron P50B03 Copolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 50% Glass Fiber Filler
Manufacturer Polyram
Trade Name Polytron
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram Polytron P50B03 Copolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A CHEMICALLY COUPLED 50% LONG GLASS FIBER REINFORCED BLACK POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.These products have significantly improved impact performance characteristics compared to other grades of Polypropylene long fiber thermoplastics. The room temperature Charpy impact properties are 25 to 30% higher at room temperature and at low temperature (-40 C). Information provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM-D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 120 MPa
17400 psi
ASTM-D638
Elongation at Break 2.1 %
2.1 %
ASTM-D638
Tensile Modulus 9.50 GPa
1380 ksi
ASTM-D790
Flexural Strength 200 MPa
29000 psi
ASTM-D790
Flexural Modulus 9.20 GPa
1330 ksi
ASTM-D790
Izod Impact, Notched 3.50 J/cm

@Temperature 23.0 °C
6.56 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 153 °C
307 °F
ASTM-D648