Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram PlusTek RD101 Nylon 12, Injection Molding

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer Polyram
Trade Name PlusTek
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek RD101 Nylon 12, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Outstanding flexibility polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
DIN 53479
Moisture Absorption at Equilibrium 0.70 %
0.70 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM-D785
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM-D638
Elongation at Break 20 %
20 %
ASTM-D638
Flexural Strength 25.0 MPa
3630 psi
ASTM D790
Flexural Modulus 0.450 GPa
65.3 ksi
ASTM-D790
Izod Impact, Notched 5.00 J/cm

@Temperature 23.0 °C
9.37 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 165 - 175 °C
329 - 347 °F
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
DIN 53482
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
DIN 53482
Dielectric Strength 55.0 kV/mm
1400 kV/in
VDE 0303/4
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved