Material Notes:
Impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
DIN 53479
Moisture Absorption at Equilibrium 2.8 %
2.8 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.013 - 0.015 cm/cm
0.013 - 0.015 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 55.0 MPa
>= 7980 psi
ASTM-D638
Elongation at Break >= 25 %
>= 25 %
ASTM-D638
Flexural Strength >= 70.0 MPa
>= 10200 psi
ASTM D790
Flexural Modulus >= 1.60 GPa
>= 232 ksi
ASTM-D790
Izod Impact, Notched >= 1.50 J/cm

@Temperature 23.0 °C
>= 2.81 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
Deflection Temperature at 0.46 MPa (66 psi) >= 150 °C
>= 302 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) >= 60.0 °C
>= 140 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in