Polyram PlusTek RB306G6 Nylon 6, 30% Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Polyram
Trade Name PlusTek
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek RB306G6 Nylon 6, 30% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% glass-fiber reinforced. Heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
DIN 53479
Water Absorption 6.6 %
6.6 %
DIN 53495
Moisture Absorption at Equilibrium 2.1 %
2.1 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.0035 cm/cm
0.0035 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM-D785
Tensile Strength, Yield 140 MPa
20300 psi
ASTM-D638
Elongation at Break 2.5 %
2.5 %
ASTM-D638
Flexural Strength 200 MPa
29000 psi
ASTM D790
Flexural Modulus 7.00 GPa
1020 ksi
ASTM-D790
Izod Impact, Notched 0.800 J/cm

@Temperature 23.0 °C
1.50 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 208 °C
406 °F
Maximum Service Temperature, Air 110 °C
230 °F
Continuous Use
200 °C
392 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 217 °C
423 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in