Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram PlusTek RB301G6 Nylon 6 for Injection Molding, 30% Glass-fiber Reinforced, Industrial Grade

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Polyram
Trade Name PlusTek
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek RB301G6 Nylon 6 for Injection Molding, 30% Glass-fiber Reinforced, Industrial Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Industrial grade, 30% glass-fiber reinforced Nylon 6 for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.90 %
0.90 %
50% RH; ISO 62
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 130 MPa
>= 18900 psi
ISO 527
Elongation at Break >= 2.0 %
>= 2.0 %
ISO 527
Flexural Strength >= 200 MPa
>= 29000 psi
ISO 178
Flexural Modulus >= 6.50 GPa
>= 943 ksi
ISO 178
Izod Impact, Notched (ISO) >= 8.00 kJ/m²
>= 3.81 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) >= 210 °C
>= 410 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) >= 190 °C
>= 374 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Flame Spread 15 mm/min
0.59 in/min
FMVSS302
Copyright © lookpolymers.com All Rights Reserved