Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram PlusTek PD502G6 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, 30% Glass Fiber Filled
Manufacturer Polyram
Trade Name PlusTek
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PD502G6 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass-fiber reinforced, V-0 1.6 mm, Nylon 12 for injection molding application.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.67 g/cc
0.0603 lb/in³
ISO 1183
Water Absorption at Saturation 1.2 %
1.2 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 115 MPa
16700 psi
ISO 527
Elongation at Break 6.0 %
6.0 %
ISO 527
Tensile Modulus 7.60 GPa
1100 ksi
ISO 527
Flexural Strength 185 MPa
26800 psi
ISO 178
Flexural Modulus 7.10 GPa
1030 ksi
ISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 165 - 175 °C
329 - 347 °F
ISO 11357
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in