Material Notes:
20% glass-fiber reinforced polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
DIN 53479
Water Absorption 1.5 %
1.5 %
DIN 53495
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
ASTM-D638
Elongation at Break 3.5 %
3.5 %
ASTM-D638
Tensile Modulus 6.00 GPa
870 ksi
ASTM-D790
Flexural Strength 140 MPa
20300 psi
ASTM D790
Flexural Modulus 4.00 GPa
580 ksi
ASTM-D790
Izod Impact, Notched 1.00 J/cm

@Temperature 23.0 °C
1.87 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 175 °C
347 °F
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in