Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram PlusTek PD120BK11 Nylon 12 for Extrusion, UV Stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, Extrusion/Tubing Grade
Manufacturer Polyram
Trade Name PlusTek
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PD120BK11 Nylon 12 for Extrusion, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 12 UV stabilized for extrusion application.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.70 %
0.70 %
50% RH; ISO 62
Water Absorption at Saturation 1.05 %
1.05 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
ISO 527
Elongation at Break 400 %
400 %
ISO 527
Tensile Modulus 1.10 GPa
160 ksi
ISO 527
Flexural Strength 30.0 MPa
4350 psi
ISO 178
Flexural Modulus 0.350 GPa
50.8 ksi
ISO 178
Izod Impact, Notched (ISO) NB
NB
ISO 180
Thermal Properties Metric English Comments
Melting Point 175 °C
347 °F
ISO 11357
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in