Material Notes:
25% glass fiber reinforced, impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
DIN 53479
Water Absorption 6.2 %
6.2 %
DIN 53495
Moisture Absorption at Equilibrium 2.0 %
2.0 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM-D785
Tensile Strength, Yield 110 MPa
16000 psi
ASTM-D638
Elongation at Break 3.0 %
3.0 %
ASTM-D638
Flexural Strength 115 MPa
16700 psi
ASTM D790
Flexural Modulus 5.50 GPa
798 ksi
ASTM-D790
Izod Impact, Notched 1.25 J/cm

@Temperature 23.0 °C
2.34 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous Use
200 °C
392 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
DIN 53482
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
DIN 53482
Dielectric Constant 6.6

@Frequency 1e+6 Hz
6.6

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 70.0 kV/mm
1780 kV/in
VDE 0303/4