Material Notes:
Flame retardant polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
DIN 53479
Water Absorption 7.6 %
7.6 %
DIN 53495
Moisture Absorption at Equilibrium 2.4 %
2.4 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.010 - 0.014 cm/cm
0.010 - 0.014 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM-D785
Tensile Strength, Yield 80.0 MPa
11600 psi
ASTM-D638
Elongation at Break 15 %
15 %
ASTM-D638
Flexural Strength 120 MPa
17400 psi
ASTM D790
Flexural Modulus 3.00 GPa
435 ksi
ASTM-D790
Izod Impact, Notched 0.500 J/cm

@Temperature 23.0 °C
0.937 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
Maximum Service Temperature, Air 90.0 °C
194 °F
Continuous Use
180 °C
356 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 185 °C
365 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
DIN 53461
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
DIN 53482
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 100 kV/mm
2540 kV/in
VDE 0303/4