Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram PlusTek PB330I6 Nylon 6 for Injection Molding, 30% Mineral and Glass-fiber Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer Polyram
Trade Name PlusTek
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PB330I6 Nylon 6 for Injection Molding, 30% Mineral and Glass-fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Mineral and glass-fiber filled, heat stabilized and low warpage Nylon 6 for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Water Absorption at Saturation 5.0 %
5.0 %
ISO 62
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa
14500 psi
ISO 527
Elongation at Break 3.5 %
3.5 %
ISO 527
Flexural Strength 150 MPa
21800 psi
ISO 178
Flexural Modulus 5.50 GPa
798 ksi
ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
ISO 11357
Maximum Service Temperature, Air 110 °C
230 °F
Continuous use
200 °C
392 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093
Dielectric Strength 90.0 kV/mm
2290 kV/in
IEC 60250
Copyright © lookpolymers.com All Rights Reserved