Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram PlusTek PB305G33BK37 Nylon 6, 33% Glass Fiber Reinforced, UV and Heat Stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Polyram
Trade Name PlusTek
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PB305G33BK37 Nylon 6, 33% Glass Fiber Reinforced, UV and Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
33% Glass fiber reinforced, UV and heat stabilized Nylon 6. Approved and listed by W.R.A.S. and NSF/ANSI 61 International for potable water.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 2.1 %
2.1 %
50% RH; ISO 62
Water Absorption at Saturation 6.6 %
6.6 %
ISO 62
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ISO 2577
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113
113
Tensile Strength, Yield 170 MPa
24700 psi
ISO 527
Elongation at Break 2.0 %
2.0 %
ISO 527
Flexural Strength 200 MPa
29000 psi
ISO 178
Flexural Modulus 5.00 GPa
725 ksi
ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
ISO 11357
Maximum Service Temperature, Air 110 °C
230 °F
Continuous use
200 °C
392 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 217 °C
423 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 3.8

@Frequency 1.00e+6 Hz
3.8

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 80.0 kV/mm
2030 kV/in
IEC 60250