Material Notes:
15% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
DIN 53479
Water Absorption 9.5 %
9.5 %
DIN 53495
Moisture Absorption at Equilibrium 3.0 %
3.0 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 120 MPa
17400 psi
ASTM-D638
Elongation at Break 2.5 %
2.5 %
ASTM-D638
Tensile Modulus 5.60 GPa
812 ksi
ASTM-D790
Flexural Strength 165 MPa
23900 psi
ASTM D790
Flexural Modulus 3.95 GPa
573 ksi
ASTM-D790
Izod Impact, Notched 0.600 J/cm

@Temperature 23.0 °C
1.12 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
Maximum Service Temperature, Air 110 °C
230 °F
Continuous Use
200 °C
392 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
DIN 53482
Dielectric Constant 3.8

@Frequency 1e+6 Hz
3.8

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 80.0 kV/mm
2030 kV/in
VDE 0303/4