Polyram PlusTek PB202G50BK39 Nylon 6, 50% Glass Fiber Reinforced, UV and Heat Stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer Polyram
Trade Name PlusTek
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PB202G50BK39 Nylon 6, 50% Glass Fiber Reinforced, UV and Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
50% Glass fiber reinforced, UV and heat stabilized Nylon 6. Approved and listed by NSF/ANSI 61 International.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.5 %
1.5 %
50% RH; ISO 62
Water Absorption at Saturation 4.8 %
4.8 %
ISO 62
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm
0.0010 - 0.0040 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 210 MPa
30500 psi
ISO 527
Elongation at Break 3.5 %
3.5 %
ISO 527
Tensile Modulus 0.0130 GPa
1.89 ksi
ISO 527
Flexural Strength 305 MPa
44200 psi
ISO 178
Flexural Modulus 13.745 GPa
1993.5 ksi
ISO 178
Izod Impact, Notched (ISO) 19.0 kJ/m²
9.04 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
ISO 11357
Maximum Service Temperature, Air 110 °C
230 °F
Continuous use
200 °C
392 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 3.8

@Frequency 1.00e+6 Hz
3.8

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 80.0 kV/mm
2030 kV/in
IEC 60250
Users viewing this material also viewed the following: