Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram PlusTek PB200 Nylon 6 for Extrusion

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Extruded
Manufacturer Polyram
Trade Name PlusTek
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PB200 Nylon 6 for Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High viscosity Nylon 6, formulated for extrusion application.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Linear Mold Shrinkage 0.013 - 0.017 cm/cm
0.013 - 0.017 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.0 MPa
9430 psi
ISO 527
Elongation at Break 65 %
65 %
ISO 527
Tensile Modulus 2.60 GPa
377 ksi
ISO 527
Flexural Modulus 2.10 GPa
305 ksi
ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 11357
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved