Material Notes:
General purpose, fast cycle Nylon 6 for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 3.0 %
3.0 %
50% RH; ISO 62
Water Absorption at Saturation 9.5 %
9.5 %
ISO 62
Linear Mold Shrinkage 0.013 - 0.017 cm/cm
0.013 - 0.017 in/in
ISO 2577
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
Tensile Strength, Yield 90.0 MPa
13100 psi
ISO 527
Elongation at Break 15 %
15 %
ISO 527
Flexural Strength 100 MPa
14500 psi
ISO 178
Flexural Modulus 2.50 GPa
363 ksi
ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
ISO 11357
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous use
180 °C
356 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 185 °C
365 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ISO 75
Flammability, UL94 V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
Glow Wire Test 850 °C
1560 °F
GWFI; IEC 60695
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 3.5

@Frequency 1.00e+6 Hz
3.5

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 100 kV/mm
2540 kV/in
IEC 60250