30% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
DIN 53479
Water Absorption 5.0 %
5.0 %
DIN 53495
Moisture Absorption at Equilibrium 1.5 %
1.5 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 145 MPa
21000 psi
ASTM-D638
Elongation at Break 3.0 %
3.0 %
ASTM-D638
Flexural Strength 210 MPa
30500 psi
ASTM D790
Flexural Modulus 6.50 GPa
943 ksi
ASTM-D790
Izod Impact, Notched 1.70 J/cm

@Temperature 23.0 °C
3.18 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
Maximum Service Temperature, Air 110 °C
230 °F
Continuous Use
>= 200 °C
>= 392 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 240 °C
464 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
DIN 53461
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
DIN 53482
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 90.0 kV/mm
2290 kV/in
VDE 0303/4