Polyram PlusTek PA320G4 Nylon 6.6, 20% Glass Fiber, Flame Retardant

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer Polyram
Trade Name PlusTek
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PA320G4 Nylon 6.6, 20% Glass Fiber, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
20% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
DIN 53479
Water Absorption 6.0 %
6.0 %
DIN 53495
Moisture Absorption at Equilibrium 1.4 %
1.4 %
50%RH; DIN 53714
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM-D785
Tensile Strength, Yield 145 MPa
21000 psi
ASTM-D638
Elongation at Break 3.0 %
3.0 %
ASTM-D638
Flexural Strength 100 MPa
14500 psi
ASTM D790
Flexural Modulus 6.70 GPa
972 ksi
ASTM-D790
Izod Impact, Notched 0.600 J/cm

@Temperature 23.0 °C
1.12 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
Maximum Service Temperature, Air 100 °C
212 °F
Continuous Use
200 °C
392 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 177 °C
350 °F
DIN 53461
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
DIN 53482
Dielectric Constant 3.8

@Frequency 1e+6 Hz
3.8

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 70.0 kV/mm
1780 kV/in
VDE 0303/4
Users viewing this material also viewed the following: