Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram PlusTek PA106 Nylon 66 for Injection Molding, with Molybdenum Disulfide

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, MoS2 Filled
Manufacturer Polyram
Trade Name PlusTek
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram PlusTek PA106 Nylon 66 for Injection Molding, with Molybdenum Disulfide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 66 with molybdenum disulfide, low friction and high abrasion resistance, for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 2.8 %
2.8 %
50% RH; ISO 62
Water Absorption at Saturation 8.5 %
8.5 %
ISO 62
Linear Mold Shrinkage 0.014 - 0.018 cm/cm
0.014 - 0.018 in/in
ISO 2577
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
Tensile Strength, Yield 90.0 MPa
13100 psi
ISO 527
Elongation at Break 15 %
15 %
ISO 527
Flexural Strength 120 MPa
17400 psi
ISO 178
Flexural Modulus 2.70 GPa
392 ksi
ISO 178
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 256 °C
493 °F
ISO 11357
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous use
200 °C
392 °F
Short peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ISO 75
Flammability, UL94 V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 3.6

@Frequency 1.00e+6 Hz
3.6

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 120 kV/mm
3050 kV/in
IEC 60250
Users viewing this material also viewed the following: