Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram BondyRam® 6000 Maleic Anhydride grafted Acrylonitrile-Butadiene-Styrene coupling agent

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , ABS Polymer
Manufacturer Polyram
Trade Name BondyRam®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram BondyRam® 6000 Maleic Anhydride grafted Acrylonitrile-Butadiene-Styrene coupling agent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Maleic Anhydride grafted Acrylonitrile-Butadiene-Styrene recommended as coupling agent in Styrene composites with glass or other minerals.Information provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D-792
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
Thermal Properties Metric English Comments
Vicat Softening Point 97.0 °C
207 °F
ASTM-D1525
Descriptive Properties Value Comments
Maleic Anhydride Level 0.7
By FTIR
Users viewing this material also viewed the following: