Polyplastic Torlen® PE 2K 901 High Density Polyethylene, Carbon Filled

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Carbon Black Filled
Manufacturer Polyplastic Group
Trade Name Torlen®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastic Torlen® PE 2K 901 High Density Polyethylene, Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyPlastic Group.
Physical Properties Metric English Comments
Density 0.942 - 0.952 g/cc
0.0340 - 0.0344 lb/in³
ISO 1183
Melt Flow 0.30 - 0.60 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 - 0.60 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
1.5 - 2.2 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.5 - 2.2 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D >= 60
>= 60
ASTM D 2240
Tensile Strength at Break 22.0 MPa
3190 psi
ASTM D 638
Tensile Strength, Yield 18.0 MPa
2610 psi
ASTM D 638
Elongation at Break 600 %
600 %
ASTM D 638
Thermal Properties Metric English Comments
Vicat Softening Point 115 °C
239 °F
ISO 306
Brittleness Temperature -70.0 °C
-94.0 °F
ASTM D 746
Processing Properties Metric English Comments
Melt Temperature 125 - 130 °C
257 - 266 °F