Polyplastic Armoflen® PO MF 65-4 Polypropylene, 65% Calcium Carbonate

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 50% Calcium Carbonate
Manufacturer Polyplastic Group
Trade Name Armoflen® PO MF
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyplastic Armoflen® PO MF 65-4 Polypropylene, 65% Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyPlastic Group.
Physical Properties Metric English Comments
Density 1.64 - 1.65 g/cc
0.0592 - 0.0596 lb/in³
ISO 1183
Particle Size 1.2 µm
1.2 µm
Melt Flow 25 - 30 g/10 min

@Load 5.00 kg,
Temperature 190 °C
25 - 30 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %