Polynorbornene Rubber (PNR)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polynorbornene Rubber (PNR).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High glass temperature - plasticizer needed to make a 'rubbery' compound.
Mechanical Properties Metric English Comments
Hardness, Shore A 15 - 95
15 - 95
Depends on compounding
Tensile Strength, Ultimate 24.0 MPa
3480 psi
Compounded Tire
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Glass Transition Temp, Tg 35.0 °C
95.0 °F