Polykemi AB SCANTEC PC 85FR Polycarbonate, Flame Retardant, Halogen Free

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant
Manufacturer Polykemi AB
Trade Name SCANTEC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB SCANTEC PC 85FR Polycarbonate, Flame Retardant, Halogen Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
With Flow; ISO 2577
0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Across Flow; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 50.0 MPa
<= 7250 psi
ISO/R527
Elongation at Yield 6.0 %
6.0 %
ISO/R527
Flexural Strength <= 95.0 MPa
<= 13800 psi
ISO 178
Flexural Modulus 2.30 GPa

@Temperature 23.0 °C
334 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 1.50 J/cm²

@Temperature -20.0 °C
7.14 ft-lb/in²

@Temperature -4.00 °F
ISO 179
2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
120°C/h; ISO 75/1
Vicat Softening Point 110 °C

@Load 5.001 kg
230 °F

@Load 11.03 lb
50°C/h; ISO 306
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Glow Wire Test 960 °C

@Thickness 2.00 mm
1760 °F

@Thickness 0.0787 in
IEC 695-2-1