Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB SCANMID 6 B60 Nylon 6, Modified

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer Polykemi AB
Trade Name SCANMID 6
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB SCANMID 6 B60 Nylon 6, Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 2.00 g/cc
0.0723 lb/in³
ISO 1183
Filler Content 60 %
60 %
±2%; Polykemi
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 73.0 MPa
<= 10600 psi
ISO/R527
Elongation at Break 5.8 %
5.8 %
ISO/R527
Elongation at Yield 5.0 %
5.0 %
ISO/R527
Flexural Strength <= 100 MPa
<= 14500 psi
ISO 178
Flexural Modulus 4.90 GPa

@Temperature 23.0 °C
711 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.350 J/cm²

@Temperature -20.0 °C
1.67 ft-lb/in²

@Temperature -4.00 °F
ISO 179
0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 190 °C
374 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C
199 °F
120°C/h; ISO 75/1
Vicat Softening Point 213 °C

@Load 5.001 kg
415 °F

@Load 11.03 lb
50°C/h; ISO 306
225 °C

@Load 1.00 kg
437 °F

@Load 2.21 lb
50°C/h; ISO 306
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved