Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
With Flow; ISO 2577
0.014 cm/cm
0.014 in/in
Across Flow; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 70.0 MPa
<= 10200 psi
ISO/R527
Elongation at Yield 5.0 %
5.0 %
ISO/R527
Flexural Strength <= 95.0 MPa
<= 13800 psi
ISO 178
Flexural Modulus 2.40 GPa

@Temperature 23.0 °C
348 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 180 °C
356 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
120°C/h; ISO 75/1
Vicat Softening Point 200 °C

@Load 5.001 kg
392 °F

@Load 11.03 lb
50°C/h; ISO 306
215 °C

@Load 1.00 kg
419 °F

@Load 2.21 lb
50°C/h; ISO 306
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
Glow Wire Test 750 °C

@Thickness 2.00 mm
1380 °F

@Thickness 0.0787 in
IEC 695-2-1