Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB SCANAMID 66 A12^ F20 FR6 Nylon 66, Glass Fiber Reinforced, Flame Retardant

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer Polykemi AB
Trade Name SCANAMID 66
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB SCANAMID 66 A12^ F20 FR6 Nylon 66, Glass Fiber Reinforced, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ISO 1183
Filler Content 20 %
20 %
±2%; Polykemi
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 150 MPa
<= 21800 psi
ISO/R527
Elongation at Break 3.0 %
3.0 %
ISO/R527
Flexural Strength <= 200 MPa
<= 29000 psi
ISO 178
Flexural Modulus 7.30 GPa

@Temperature 23.0 °C
1060 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Copyright © lookpolymers.com All Rights Reserved