Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB POLYshine PBT D311 GF30 PBT, Glass-Fiber Reinforced, Modified

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer Polykemi AB
Trade Name POLYshine
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYshine PBT D311 GF30 PBT, Glass-Fiber Reinforced, Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
Filler Content 30 %
30 %
±2%; Polykemi
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
0.0080 cm/cm
0.0080 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 145 MPa
<= 21000 psi
ISO/R527
Elongation at Break 3.0 %
3.0 %
ISO/R527
Flexural Strength <= 180 MPa
<= 26100 psi
ISO 178
Flexural Modulus 7.80 GPa

@Temperature 23.0 °C
1130 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.700 J/cm²

@Temperature -20.0 °C
3.33 ft-lb/in²

@Temperature -4.00 °F
ISO 179
0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
120°C/h; ISO 75/1
Vicat Softening Point 215 °C

@Load 5.001 kg
419 °F

@Load 11.03 lb
50°C/h; ISO 306
Users viewing this material also viewed the following: