Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB POLYshine PBT D201 T20 PBT, Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Polykemi AB
Trade Name POLYshine
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYshine PBT D201 T20 PBT, Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
Filler Content 20 %
20 %
±2%; Polykemi
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 50.0 MPa
<= 7250 psi
ISO/R527
Elongation at Break 16 %
16 %
ISO/R527
Elongation at Yield 5.0 %
5.0 %
ISO/R527
Flexural Strength <= 92.0 MPa
<= 13300 psi
ISO 178
Flexural Modulus 4.40 GPa

@Temperature 23.0 °C
638 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.300 J/cm²

@Temperature -20.0 °C
1.43 ft-lb/in²

@Temperature -4.00 °F
ISO 179
0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 113 °C
235 °F
120°C/h; ISO 75/1
Vicat Softening Point 187 °C

@Load 5.001 kg
369 °F

@Load 11.03 lb
50°C/h; ISO 306
Glow Wire Test 650 °C

@Thickness 2.20 mm
1200 °F

@Thickness 0.0866 in
IEC 695-2-1
Copyright © lookpolymers.com All Rights Reserved