Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB POLYshine PBT D201 FB60 PBT, Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Polykemi AB
Trade Name POLYshine
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYshine PBT D201 FB60 PBT, Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 2.00 g/cc
0.0723 lb/in³
ISO 1183
Filler Content 60 %
60 %
±2%; Polykemi
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 100 MPa
<= 14500 psi
ISO/R527
Elongation at Break 4.0 %
4.0 %
ISO/R527
Flexural Strength <= 150 MPa
<= 21800 psi
ISO 178
Flexural Modulus 12.0 GPa

@Temperature 23.0 °C
1740 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.500 J/cm²

@Temperature -20.0 °C
2.38 ft-lb/in²

@Temperature -4.00 °F
ISO 179
0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
410 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
120°C/h; ISO 75/1