Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB POLYlux 4010 MP PC/PBT-Blend

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Polykemi AB
Trade Name POLYlux
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYlux 4010 MP PC/PBT-Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
With Flow; ISO 2577
0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
Across Flow; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 50.0 MPa
<= 7250 psi
ISO/R527
Flexural Strength <= 80.0 MPa
<= 11600 psi
ISO 178
Flexural Modulus 2.00 GPa

@Temperature 23.0 °C
290 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
NB

@Temperature -20.0 °C
NB

@Temperature -4.00 °F
ISO 179
Charpy Impact, Notched 4.00 J/cm²

@Temperature -20.0 °C
19.0 ft-lb/in²

@Temperature -4.00 °F
ISO 179
4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
120°C/h; ISO 75/1
Vicat Softening Point 120 °C

@Load 5.001 kg
248 °F

@Load 11.03 lb
50°C/h; ISO 306