Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB POLYlux 3809S FR PC/PBT-Blend, Flame Retardant

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Polykemi AB
Trade Name POLYlux
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYlux 3809S FR PC/PBT-Blend, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 40.0 MPa
<= 5800 psi
ISO/R527
Elongation at Yield 5.0 %
5.0 %
ISO/R527
Flexural Strength <= 67.0 MPa
<= 9720 psi
ISO 178
Flexural Modulus 2.30 GPa

@Temperature 23.0 °C
334 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 179
1.30 J/cm²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
120°C/h; ISO 75/1
Vicat Softening Point 110 °C

@Load 5.001 kg
230 °F

@Load 11.03 lb
50°C/h; ISO 306
134 °C

@Load 1.00 kg
273 °F

@Load 2.21 lb
50°C/h; ISO 306
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Users viewing this material also viewed the following: