Polykemi AB POLYlux 3809S F20 PC/PBT-Blend, Glass Fiber-Reinforced

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Polykemi AB
Trade Name POLYlux
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYlux 3809S F20 PC/PBT-Blend, Glass Fiber-Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Filler Content 20 %
20 %
±2%; Polykemi
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
With Flow; ISO 2577
0.0080 cm/cm
0.0080 in/in
Across Flow; ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 80.0 MPa
<= 11600 psi
ISO/R527
Elongation at Break 4.0 %
4.0 %
ISO/R527
Flexural Modulus 4.80 GPa

@Temperature 23.0 °C
696 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
120°C/h; ISO 75/1
Vicat Softening Point 125 °C

@Load 5.001 kg
257 °F

@Load 11.03 lb
50°C/h; ISO 306