Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Polykemi AB
Trade Name POLYlux
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYlux 104 HF PC/PBT-Blend, High Flow.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 56.0 MPa
<= 8120 psi
ISO/R527
Elongation at Yield 8.0 %
8.0 %
ISO/R527
Flexural Strength <= 95.0 MPa
<= 13800 psi
ISO 178
Flexural Modulus 2.10 GPa

@Temperature 23.0 °C
305 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 3.30 J/cm²

@Temperature -20.0 °C
15.7 ft-lb/in²

@Temperature -4.00 °F
ISO 179
4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 118 °C
244 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
120°C/h; ISO 75/1
Vicat Softening Point 124 °C

@Load 5.001 kg
255 °F

@Load 11.03 lb
50°C/h; ISO 306
148 °C

@Load 1.00 kg
298 °F

@Load 2.21 lb
50°C/h; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in