Polykemi AB POLYelast TPE Z805P Thermoplastic Elastomer, SEBS-based

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Polykemi AB
Trade Name POLYelast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYelast TPE Z805P Thermoplastic Elastomer, SEBS-based.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Linear Mold Shrinkage 0.014 - 0.020 cm/cm
0.014 - 0.020 in/in
With Flow; ISO 2577
0.014 - 0.020 cm/cm
0.014 - 0.020 in/in
Across Flow; ISO 2577
Mechanical Properties Metric English Comments
Hardness, Shore A 80

@Time 15.0 sec
80

@Time 0.00417 hour
Polykemi
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Back Pressure 0.500 - 1.50 MPa
72.5 - 218 psi
Descriptive Properties Value Comments
Holding Pressure () Low
% of injection pressure
Injection Pressure Low
Injection Speed () High