Polykemi AB POLYelast TPE Z600A Thermoplastic Elastomer, SEBS-based, Co-injection Grade

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Polykemi AB
Trade Name POLYelast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYelast TPE Z600A Thermoplastic Elastomer, SEBS-based, Co-injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.00 g/cc
0.0361 lb/in³
ISO 1183
Linear Mold Shrinkage 0.017 - 0.024 cm/cm
0.017 - 0.024 in/in
With Flow; ISO 2577
0.017 - 0.024 cm/cm
0.017 - 0.024 in/in
Across Flow; ISO 2577
Mechanical Properties Metric English Comments
Hardness, Shore A 60

@Time 15.0 sec
60

@Time 0.00417 hour
Polykemi
Tensile Strength at Break <= 10.0 MPa
<= 1450 psi
ISO/R527
Elongation at Break 700 %
700 %
ISO/R527
100% Modulus 0.00240 GPa
0.348 ksi
ISO/R527
300% Modulus 0.00320 GPa
0.464 ksi
ISO/R527
Tear Strength 25.0 kN/m
143 pli
D624
Processing Properties Metric English Comments
Melt Temperature 200 - 220 °C
392 - 428 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Dry Time 1 - 2 hour
1 - 2 hour
in desiccant air dryer
Back Pressure 0.500 - 1.50 MPa
72.5 - 218 psi
Descriptive Properties Value Comments
Holding Pressure () Low
% of injection pressure
Injection Pressure Low
Injection Speed () High