Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Linear Mold Shrinkage 0.015 - 0.022 cm/cm
0.015 - 0.022 in/in
With Flow; ISO 2577
0.015 - 0.022 cm/cm
0.015 - 0.022 in/in
Across Flow; ISO 2577
Mechanical Properties Metric English Comments
Hardness, Shore A 60

@Time 15.0 sec
60

@Time 0.00417 hour
Polykemi
Tensile Strength at Break <= 5.00 MPa
<= 725 psi
ISO/R527
Elongation at Break 425 %
425 %
ISO/R527
100% Modulus 0.00250 GPa
0.363 ksi
ISO/R527
300% Modulus 0.00350 GPa
0.508 ksi
ISO/R527
Tear Strength 25.0 kN/m
143 pli
D624
Processing Properties Metric English Comments
Melt Temperature 180 - 205 °C
356 - 401 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Descriptive Properties Value Comments
Back Pressure Medium
Holding Pressure () Low
% of injection pressure
Injection Pressure High
Injection Speed () Low-Medium