Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB POLYblend 6005B PC/ABS-Blend

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Polykemi AB
Trade Name POLYblend
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYblend 6005B PC/ABS-Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0080 - 0.010 cm/cm
0.0080 - 0.010 in/in
With Flow; ISO 2577
0.0080 - 0.010 cm/cm
0.0080 - 0.010 in/in
Across Flow; ISO 2577
Melt Index of Compound 14 g/10 min

@Load 5.00 kg,
Temperature 240 °C
14 g/10 min

@Load 11.0 lb,
Temperature 464 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 62

@Time 15.0 sec
62

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break <= 45.0 MPa
<= 6530 psi
ISO/R527
Elongation at Break >= 80 %
>= 80 %
ISO/R527
Flexural Strength <= 60.0 MPa
<= 8700 psi
ISO 178
Flexural Modulus 1.80 GPa

@Temperature 23.0 °C
261 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 5.00 J/cm²

@Temperature 23.0 °C
23.8 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C
205 °F
120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C
126 °F
120°C/h; ISO 75/1
Vicat Softening Point 110 °C

@Load 5.001 kg
230 °F

@Load 11.03 lb
50°C/h; ISO 306
190 °C

@Load 1.00 kg
374 °F

@Load 2.21 lb
50°C/h; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Glow Wire Test 650 °C

@Thickness 2.00 mm
1200 °F

@Thickness 0.0787 in
IEC 695-2-1
Users viewing this material also viewed the following: