Polyimide Fiber

Category Other Engineering Material , Composite Fibers , Polymer , Thermoset , Polyimide, TS
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyimide Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 830 MPa
120000 psi
Modulus of Elasticity 2.80 GPa
406 ksi