Polycasa SPC UK Polycarbonate Multiwall Sheet

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Polycasa
Trade Name SPC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polycasa SPC UK Polycarbonate Multiwall Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
QUINN SPC UK has variety of characteristics and benefits includingHigh impact resistanceWeather resistantHigh heat and sound insulationLong life spanExcellent light transmissionTransparentResistant to chemicalsLight WeightSuperb thermal insulationRoofing and glazing Swimming pool enclosures Cladding Conservatories Skylights Boxes Shelters Protective covers for fragile items Vaults Advertising panels Suspended ceilings Winter gardens Partitions PergolasQuinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013.
Physical Properties Metric English Comments
Apparent Bulk Density 0.140 g/cc
0.00506 lb/in³
25 mm - 5 wall
0.170 g/cc
0.00614 lb/in³
10 mm - 2 wall
Thermal Properties Metric English Comments
Thermal Conductivity 0.0290 W/m-K
0.201 BTU-in/hr-ft²-°F
10 mm - 2 wall
0.0425 W/m-K
0.295 BTU-in/hr-ft²-°F
25 mm - 5 wall
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Optical Properties Metric English Comments
Transmission, Visible 14 %
14 %
Opal, 25mm - 5 wall
17 %
17 %
Bronze Opal, 25mm - 5 wall
17 %
17 %
Bronze, 25mm - 5 wall
37 %
37 %
Bronze, 10mm - 2 wall
45 %
45 %
Opal, 10mm - 2 wall
62 %
62 %
Clear, 25mm - 5 wall
88 %
88 %
Clear, 10mm - 2 wall
UV Transmittance 34 %
34 %
Opal, 25mm - 5 wall
39 %
39 %
Bronze, 25mm - 5 wall
40 %
40 %
Bronze Opal, 25mm - 5 wall
63 %
63 %
Clear, 25mm - 5 wall