Material Notes:
Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of thermoplastics. These materials provide the benefits of proprietary conductive additive technologies and the performance of select engineering thermoplastic resins. Therma-Tech compounds have been shown to improve thermal conductivity up to 100-times that of conventional plastics and can be used in a wide range of thermal management applications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.60 g/cc
1.60 g/cc
ASTM D792
Water Absorption 0.50 %

@Thickness 3.18 mm
0.50 %

@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.3 MPa
7010 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 0.80 %
0.80 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 14.5 GPa
2100 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 89.6 MPa
13000 psi
ASTM D790
Flexural Modulus 11.0 GPa
1600 ksi
ASTM D790
Izod Impact, Notched 0.210 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.393 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Thermal Conductivity 11.0 W/m-K
76.3 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 260 °C

@Thickness 6.35 mm
500 °F

@Thickness 0.250 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 254 °C

@Thickness 6.35 mm
489 °F

@Thickness 0.250 in
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1000 - 10000 ohm-cm
1000 - 10000 ohm-cm
ASTM D257
Surface Resistance 100 - 1000 ohm
100 - 1000 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 282 - 299 °C
540 - 570 °F
Mold Temperature 65.6 - 93.3 °C
150 - 200 °F
Descriptive Properties Value Comments
Features Electrically Conductive
Thermally Conductive
Forms Pellets
Generic Material Nylon 66
Generic Name Polyamide 66 (Nylon 66)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Automotive Under the Hood
Consumer Applications
Electrical/Electronic Applications
Housings
Industrial Applications
Users viewing this material also viewed the following: