PolyOne Synprene® ST-6250 Thermoplastic Elastomer - SBC  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® ST-6250 Thermoplastic Elastomer - SBC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Over-Molding GradeUV StabilizedApplications:Multi-PurposeProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792
Linear Mold Shrinkage 0.020 cm/cm
0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
5 sec; ASTM D2240
Tensile Strength, Yield 6.07 MPa
880 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
1.83 MPa

@Strain 100 %
265 psi

@Strain 100 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
3.72 MPa

@Strain 300 %
540 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 615 %
615 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 28.0 kN/m
160 pli
Die C (graves), 20 in/min; ASTM D624