PolyOne Synprene® RT-3760 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® RT-3760 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection MoldingInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 63
63
Instant; ASTM D2240
Tensile Strength, Yield 5.31 MPa
770 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
2.34 MPa

@Strain 300 %
340 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 700 %
700 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Rebound 38 %
38 %
Bayshore; ASTM D2632
Tear Strength 23.3 kN/m
133 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 24 %
24 %
Method B, 73°F(23°C), 22 hrs; ASTM D395