Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Synprene® RT-3740 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® RT-3740 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
1.18 g/cc
1.18 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 43
43
Instant; ASTM D2240
53
53
Instant; ASTM D2240
Tensile Strength, Yield 4.00 MPa
580 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
4.69 MPa
680 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
1.41 MPa

@Strain 300 %
205 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
2.07 MPa

@Strain 300 %
300 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 750 %
750 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
800 %
800 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Rebound 40 %
40 %
Bayshore; ASTM D2632
40 %
40 %
Bayshore; ASTM D2632
Tear Strength 15.8 kN/m
90.0 pli
Die C (graves), 20 in/min; ASTM D624
20.2 kN/m
115 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 15 %
15 %
Method B, 73°F(23°C), 22 hrs; ASTM D395
20 %
20 %
Method B, 73°F(23°C), 22 hrs; ASTM D395
Users viewing this material also viewed the following: