PolyOne Synprene® RT-3620 Thermoplastic Elastomer - SBC  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® RT-3620 Thermoplastic Elastomer - SBC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 20
20
Instant; ASTM D2240
Tensile Strength, Yield 2.55 MPa
370 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
0.931 MPa

@Strain 300 %
135 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 730 %
730 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 10.5 kN/m
60.0 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 12 %
12 %
Method B, 73°F(23°C), 22 hrs; ASTM D395